Bare cadmium free low temperature silver brazing alloy.
A cadmium free food grade brazing alloy with low melting temperature. For joining and repair of steels, stainless steels, nickel, copper, and high speed steels. Use with All-State No. 110 flux or All-State S-200 flux 56% Silver

| Part No. | Model / Product Description | UPC |
|---|---|---|
| 69050272 | A/S 155 1/16X18X1# TUBE | 662393003008 |
| 69050273 | A/S 155 3/32X18X1# TUBE | 662393003015 |
| 69050276 | A/S 155 SILV DISP 2 OZ X 12 | 662393003022 |
| 69050277 | A/S 155 1/16X18X4OZ | 662393003039 |
| 69050278 | A/S 155B 3/32X18X4 OZ TUBE | 662393003046 |
| 69050307 | A/S 155 1/16X1XCL | 662393003107 |
| 69050324 | A/S 155BA PASTE 3OZ SYRINGE | 662303065478 |
Thoroughly clean joint area. Joint clearance should be .002" to .005". Apply All-State No. 110 or S-200 Flux to joint; if necessary, thin with alcohol or water. When working on stainless steel and other materials subject to discoloration, paint area adjacent to joint with All-State No. 110 or S-200 Flux. Apply heat with a slightly carburizing flame until flux turns clear. Melt off enough alloy to fill completely. Allow to cool slowly. Remove flux with hot water.