A 56% silver content, low temperature, cadmium free, food/medical grade brazing alloy. Excellent capillary flow on ferrous and nonferrous metals (except white metals) or combinations of both. Use on steel, stainless steel, nickel or copper and their alloys. Typically uses are brewery, bottling plant, laboratory or food packaging equipment. Use 110 or S-200 Flux when using 155 bare.
A cadmium free food grade brazing alloy with low melting temperature. For joining and repair of steels, stainless steels, nickel, copper, and high speed steels. Use with All-State No. 110 flux or All-State S-200 flux 56% Silver

| Typical Mechanical Properties | |
|---|---|
| Tensile Strength | Up to 50 ksi, 35.16 kgs/mm2 |
| Working Temperature | 1150-1200 °F, 621-649 °C |
| Corrosion Resistance | Good |
Maintenance and production joining and repairing of steels, stainless steels, nickel and nickel base metals, copper and copper base alloys and high speed steels where high brazing temperatures would be harmful. Widely used in hospitals, laboratories, distilleries, refineries and delicate instrumentation work.
Thoroughly clean joint area. Joint clearance should be .002" to .005". Apply All-State No. 110 or S-200 Flux to joint; if necessary, thin with alcohol or water. When working on stainless steel and other materials subject to discoloration, paint area adjacent to joint with All-State No. 110 or S-200 Flux. Apply heat with a slightly carburizing flame until flux turns clear. Melt off enough alloy to fill completely.Allow to cool slowly. Remove flux with hot water.
All listed prices are in U.S. dollars and represent the Manufacturer's Suggested Retail Price (MSRP) for sale in the United States. Actual selling price will be determined by the Distributor. Prices are subject to change without notice.