Cadmium free general purpose silver brazing alloy.
45% silver brazing alloy for use on light gauge material and tight fitting joints. Excellent capillary flow on ferrous and non-ferrous metals or combinations of both (excluding white metals). Excellent for food processing or food handling equipment. Use with All-State No. 110 or All-State S-200 flux.

| Typical Mechanical Properties | |
|---|---|
| Tensile Strength | up to 75 ksi |
| Working Temperature | 1225-1370 °F, 663-743 °C |
| Corrosion Resistance | Good |
| Part No. | Model / Product Description | UPC |
|---|---|---|
| 69050178 | A/S 101 CD FR SIL DSP 2OZX12 | 662393519882 |
| 69050179 | A/S 101 CD FR SIL DSP 4OZX12 | 662393519899 |
| 69050243 | A/S 101 CD FR 1/16X18X4OZ | 662393519851 |
| 69050244 | A/S 101 CD FR 3/32X18X4OZ | 662393519868 |
| 69050352 | A/S 101 CD FR 1/16X2 OZ CL | 662393010662 |
| 69050353 | A/S 101 CD FR 1/16X4 OZ CL | 662303065485 |
| 69050354 | A/S 101 CD FR 1/16X1XCOIL | 662393519844 |
| 69050400 | A/S 101 CD FR 1/16X18X1# TUBE | 662393054925 |
| 69050401 | A/S 101 CD FR 3/32X18X1#T | 662393668320 |
| 69050402 | A/S 101 CD FR 1/8X18X1#TUBE |
Recommended maximum operating temperature is up to 400°F (204ºC) in continuous service and up to 600°F (315ºC) for intermittent service.