Print this page

ALL-STATE 100

A cadmium free nickel bearing food grade silver brazing alloy for stainless steel, carbide tools, and for joining ferrous and nonferrous metals (except white metals) 40% Silver.

Features

A cadmium free nickel bearing food grade silver brazing alloy for stainless steel, carbide tools, and for joining ferrous and nonferrous metals (except white metals) 40% Silver.

Classifications

Properties

Typical Properties
Typical Mechanical Properties  
Tensile Strength Up to 60 ksi, 42.19 kgs/mm2
Working Temperature 1250-1400 °F, 677-760 °C
Corrosion Resistance Very Good

Part No.

100
Part No. Model / Product Description UPC
69050201 A/S 100 1/16X2OZ COIL 662393002841
69050209 A/S SILFLO 40 R&R 1/16X4 OZ CL 662393002889
69050174 A/S 100 SIL DSP 2 OZ X 12 662393002766
69050197 A/S 100 3/32X18X1# TUBE 662393002834
69050204 A/S 100 1/16X18X4OZ TUBE 662393002858
69050205 A/S 100 3/32X18X4OZ TUBE 662393002865
69050207 A/S 100 1/16X18X1# TUBE 662393002872
69050218 A/S 100 1/32X1# SPL 662393009277
69050300 A/S 100 1/16X1XCOIL 662393003077

SAW

Accessories

Depositions/Paramaters

Extra Info

Brazing carbide tool assemblies, joining parts subjected to corrosive materials and atmospheres, fabricating and repairing stainless steel food handling equipment, and joining ferrous and non-ferrous materials (excluding the white metals.)

Procedure

Thoroughly clean area to be brazed. Recommended joint clearance is .002" to .005". Paint joint area with All-State No. 110 or S-200 Flux reduced with water or alcohol if necessary. With a slightly carburizing flame heat joint rapidly and uniformly keeping torch in constant motion. Allow to cool slowly and then remove flux residue with warm water.