A copper coated, mild steel TIG rod with good wetting characteristics and excellent bead appearance. Has excellent tolerance for rust and mill scale. Use for butt and fillet welds. Applications: HVAC duct work and carbon steels.
A mild steel, copper coated TIG rod with good wetting characteristics, and excellent bead appearance. Can be used on uncleaned metal.

| Typical Mechanical Properties | |
|---|---|
| As Welded | |
| Yield Strength | 68 ksi, 468 kgs/mm2 |
| Tensile Strength | 86 ksi, 592 kgs/mm2 |
| Elongation in 2" | 26 % |
| Reduction in Area | 58 % |
| Stress Relieved 8 hrs. @ 1150°F (621°C) | |
| Yield Strength | 64 ksi, 441 kgs/mm2 |
| Tensile Strength | 80 ksi, 551 kgs/mm2 |
| Elongation in 2" | 29 % |
| Reduction in Area | 68 % |
| Charpy V-Notch Impact Properties | |
| Stress Relieved 2 hrs. @ 1150°F (621°C) | |
| @ -20°F | 48 ft.-lbs. |
| Stress Relieved 8 hrs. @ 1150°F (621°C) | |
| @ 50°F | 28 ft.-lbs. |