Stainless steel electrode for welding 316L and 318 type steels.
Used for welding 316L and 318 type steels. Weld deposit has a maximum of .04% carbon. Widely used in the chemical industry.

| Part No. | Model / Product Description | UPC |
|---|---|---|
| 69118336 | A/S 316L-16 ACDC 3/32X9X6#HSC | 662393011355 |
| 69122116 | A/S 316L-16 ACDC 1/16X9X6#HS | 662393011072 |
| 69122180 | A/S 316L-16 ACDC 1/8X14X10# | 662393005200 |
| 69122530 | A/S 316L-16 ACDC 5/32X14X10# | 662393519783 |
| 69001023 | A/S *316-16 1/8 DISPLAY PACK | 662303065584 |
| 69122336 | A/S 316L-16 ACDC 3/32X9X6#HS | 662393519776 |