All-position DC reverse flux cored stainless steel wire.
All-position, DC reverse, flux cored stainless steel wire with self-peeling slag. Designed for welding stainless 304 to mild or carbon steel, 309 wrought or cast forms, 304 clad sheets, and for applying stainless steel sheet linings to carbon steel. For best results, use with a 75% Argon/25% CO2 shielding gas. Meets AWS A5.22,Class E309LT-1

| Typical Mechanical Properties | |
|---|---|
| As Welded 75% Ar / 25% CO2 | |
| Yield Strength | 66 ksi, 459 N/mm2 |
| Tensile Strength | 84 ksi, 589 N/mm2 |
| Elongation In 2" | 37 % |
The choice for welding mild steel to stainless steel. Excellent corrosion resistant properties on 309 alloys at room termperatures and oxidation resistance up to 2000°F. Ideal for overlay and buildup work.Use on 309 (wrought or cast form), 304 clad stainless steels, air hardening steels where heat treating is not necessary, and low alloy steels.
All listed prices are in U.S. dollars and represent the Manufacturer's Suggested Retail Price (MSRP) for sale in the United States. Actual selling price will be determined by the Distributor. Prices are subject to change without notice.