Print this page

ALL-STATE RG-65

A bare rod for braze welding of tubes, pipes, sheets, pressure vessels and tanks in the 65-75 ksi range. Provides higher weld strengths on low alloy steels.

Features

(Bare Finish) For oxy-fuel welding of tubes, pipes, sheets,pressure vessels, and tanks in the 65-75 ksi range. Higher weld strengths on low alloy steels. Meets AWS A5.2, Class R65

Classifications

Properties

Typical Properties
Typical Mechanical Properties  
Tensile Strength  
As Welded 70-80 ksi, 486-551 kgs/mm2
Heat Treated 200 ksi

Part No.

RG-65
Part No. Model / Product Description UPC
69700310 A/S RG-65 1/16X36X50# 662393007112
69700312 A/S RG-65 3/32X36X50# 662393007129
69700314 A/S RG-65 1/8X36X50# 662393007136
69700316 A/S RG-65 5/32X36X50# 662393520055
69710310 A/S RG-65 1/16X36X5X30# 662393007471
69710312 A/S RG-65 3/32X36X5X30# 662393007488
69710314 A/S RG-65 1/8X36X5X30# 662393007495

SAW

Accessories

Depositions/Paramaters

Extra Info

RG-65 is a low alloy steel rod used for high speed fusion welding of pressure vessels, tanks and pipe.

Procedure

Clean joint area. Bevel heavy sections. Adjust torch to neutral flame. Keep torch tip at low angle to base metal. Preheat normally not necessary.

Complementary Products

Seismic Data