ALL-STATE® Cutting Rod

Electrode for cutting and piercing of all metals.

Features

An AC/DC straight, all-position electrode for cutting and piercing of all metals.

Classifications

Properties

Typical Properties

Part No.

Cutting Rod
Part No. Model / Product Description UPC
69010118 A/S CTG ELEC 1/8X14X5X40 662393000519
69010119 A/S CTG ELEC 5/32X14X5X40 662393000526
69010120 A/S CTG ELEC 3/16X14X5X40 662393000533
69010121 A/S CTG ELEC 1/8X14X50#CT 662393000540
69010122 A/S CTG ELEC 5/32X14X50 662393000557
69010123 A/S CTG ELEC 3/16X14X50 UTD 662393000564
69010124 A/S CTG ELEC 1/4X18X50 662393000571

SAW

Accessories

Depositions/Paramaters

Extra Info

All-State Cutting Electrode will cut without the use of oxygen or compressed air. This electrode is designed to have a slow burn off rate with a special coating that produces exothermic heat which gives more inches of cutting per electrode. Cutting nickel, copper, brass, bronze, cast iron, stainless steel, aluminum, carbon and alloy steels. Piercing holes, removing rivets, bolts, and defects in any of the above materials.

Procedure

Clean cuts can be made by using either an AC or DC machine of sufficient capacity. A DC machine set on straight polarity will give the best results. To cut through a piece of metal, it will be easier if it is placed in the flat position. Hold the electrode at a 75 degree angle to the piece to be cut. Strike the arc and using the electrode as if it were a hand saw, keep the end of the electrode in constant contact with the work and continue with the sawing action. A short arc must be maintained to produce a clean cut and reduce overheating of the workpiece. Piercing holes is very easy. Hold the electrode in the vertical position, strike an arc and push the electrode down until it penetrates through the material. Manipulate the electrode in a sawing motion to enlarge the hole.