ALL-STATE OVERLAY 5862

Metal cored hardfacing wire for abrasion.

Features

A high carbon, chromium carbide, metal-cored, open-arc hardfacing wire for abrasion and abrasion with mild impact on tillage tools, blades, paddles, chutes and teeth. Slag free deposits cannot be flame-cut. Deposit hardness 58-62 RC.

Classifications

Properties

Typical Properties
Typical Mechanical Properties  
Hardness 58-62 Rc

Part No.

OVERLAY 5862
Part No. Model / Product Description UPC
69870464 A/S OVERLAY 5862 045X25# SP 662393065297
69870471 A/S OVERLAY 5862 1/16X25# SP 662393065334

SAW