ALL-STATE OVERLAY 4550

Metal-cored, gas-shielded hard-surfacing wire.

Features

Metal-cored, gas-shielded, Argon/CO2 75/25 or Argon Oxygen 98/2 hard-surfacing wire. Tough, shock resistant, tool steel type wire offers good corrosion resistance, excellent metal-to-metal wear and abrasion characteristics. Deposits polish in-service to reduce friction and minimize wear of mating parts. Excellent resistance to heat checking. Multi-layer,crack-free deposits. Deposit hardness 45-50 RC

Classifications

Properties

Typical Properties
Typical Mechanical Properties  
Hardness 45-50 Rc

Part No.

OVERLAY 4550
Part No. Model / Product Description UPC
69870458 A/S OVERLAY 4550 045X25#SPL 662393009635

SAW

Accessories

Depositions/Paramaters

Extra Info

Typical applications: Forging dies, ingot buggy car wheels, kiln trunnions, steel mill rolls, cable sheaves, dredge ladder rolls, and overlaying of shafts. For use on carbon, stainless and manganese steels.

Procedure

Clean base metal and preheat according to type of steel.