ALL-STATE ROLL MATRIX

Completely machinable deposit for heavy impact and compression on abrasion resistant, carbon and low alloy steels.

Features

Completely machinable deposit for heavy impact and compression on abrasion resistant, carbon and low alloy steels. Deposits have excellent toughness and resistance to deformation. They can be forged and flame cut and will respond to heart treatment. Ideal for tractor pads and rollers, sprockets, idlers, hammers, wobblers, excavators, shafts, gear teeth, steel mill roll necks and ends, and all carbon steel parts requiring build-up prior to hardsurfacing.

Classifications

Properties

Typical Properties
Typical Mechanical Properties  
Tensile Strength up to 105 ksi, 73.84 kgs/mm2
Hardness (Rockwell) 25 to 30 Rc

Part No.

OVERLAY Roll Matrix
Part No. Model / Product Description UPC
69011502 A/S ROLL MATRIX 1/8X14X1#T 662393014493

SAW

Accessories

Depositions/Paramaters

Extra Info

Procedure

Clean weld area. Use All-State® Chamfer Rod to remove fatigued or damaged metal. Preheat is
usually not necessary but heavy sections may require a preheat of 200°-300°F (93°-149°C).
Hold a short to medium arc length. Remove all slag between passes. Use stringer or weave
beads. Do not allow excessive heat build-up. Allow part to cool slowly.