A superior electrode with high tungsten content that, along with other elements, form a bead of complex carbides. Use in extreme wet or dry sliding abrasion or corrosion. Build-up: 2 passes maximum.
A highly alloyed AC/DC reverse electrode for superior wear resistance involving extreme abrasion. Hardness up to 63-67 Rockwell C.

| Typical Mechanical Properties | |
|---|---|
| Hardness | 65-67 Rc |
Ideal for components and parts operating under extremely severe conditions experienced by earth moving equipment and wear resisting parts in cement mills and brick manufacturing.
Stringer beads recommended. Remove slag prior to making next weld. Hold the electrode over the weld puddle instead of slightly in front of it.