ALL-STATE Paste Solder

A 50/50 lead/tin solder for sealing, joining or tinning most metals except aluminum. Not for food or medical use.

Features

A 50/50 lead/tin solder for sealing, joining or tinning most common metals, except aluminum. Can be used with soldering iron or torch. Working temperature is 360°F to 375°F.

Classifications

Properties

Typical Properties
Typical Mechanical Properties  
Tensile Strength Up to 6 ksi, 4.57 kgs/mm2
Solidus 360 °F, 182 °C
Liquidus 375 °F, 191 °C

Part No.

Paste Solder
Part No. Model / Product Description UPC
69070060 A/S PASTE SOLDER 1#X12 662393003817

SAW

Accessories

Depositions/Paramaters

Extra Info

Soldering can be confined to a desired area, thus saving material, labor and equipment. The active flux contained in this compound eliminates problems of application to difficult or hard-to-reach areas. It may be easily brushed or spotted in place. Recommended for multiple wire assemblies, repairing radiators, internal tinning, air conditioning, auto body tinning and repair, and costume jewelry assembly.

Procedure

Clean area to be joined. Apply thin coat of All-State Paste Solder to the joint. Maintain a tight joint by using a fixture or a clamp. Heat with a soldering iron, torch, furnace, induction heater or any source capable of producing 375°F (181°C) Allow the soldered part to cool before attempting to move and wash off black flux residue with hot water.