ALL-STATE JET FLUX

Liquid flux used in jet flux system.

Features

Clear liquid welding and brazing flux for use on steels, copper, and cast iron with the All-State Jet Fluxing system. Active from 1400°F to 1800°F. Flammable,performs to MIL-F-16135B

Classifications

Properties

Typical Properties

Part No.

Jet Flux
Part No. Model / Product Description UPC
69080172 A/S JET FLUX 53 GAL DRUM 662393004012
69080171 A/S JET FLUX 5 GAL 662393004005
69080170 A/S JET FLUX 1 GAL 662393003992