ALL-STATE 1113

Paste flux for high temperature brazing on cast iron, mild steel, nickel silvers and copper.

Features

Gray paste flux for welding and brazing on cast iron, mild steel, nickel silvers, and copper. Active from 1400°F and protects up to 2200°F. Performs to AWS A5.31,Type FB3-G

Classifications

Properties

Typical Properties

Part No.

1113
Part No. Model / Product Description UPC
69080034 A/S BRAZO 1113 FLUX 35# PAIL 662393009796
69080227 A/S 1113 NCK SILVER FLUX 1X1 662393004227