ALL-STATE S-200 FLUX

Silver brazing formula flux.

Features

White paste brazing flux for stainless steels, monel, copper alloys, and silver alloys. Active at 1100°F and protects to 1800°F. Performs to AWS A5.31, Type FB3-A, AMS 3410F, Mil-F-4483, and Fed OF499D.

Classifications

Properties

Typical Properties

Part No.

S-200
Part No. Model / Product Description UPC
69080218 A/S S-200 FLUX 8 0Z X 12 662393004166