ALL-STATE 110 FLUX

Flux for brazing stainless steel, nickel, monel, copper bearing alloys and silver bearing alloys.

Features

Blue paste brazing flux for stainless steel, nickel, monel, copper alloys, and silver alloys. Active at 1000°F protects up to 1600°F. Performs to AWS A5.31, Type FB3-A, AMS 3410F, Mil-F-4483, and Fed OF499D.

Classifications

Properties

Typical Properties

Part No.

110
Part No. Model / Product Description UPC
69080215 A/S 110 FLUX 7 OZ X 12 662393004135
69080216 A/S 110 FLUX 8 OZ X 12 662393004142
69080217 A/S 110 FLUX 1# X 12 662393004159