Flux for brazing on steel, cast iron, copper and brass.
White powder flux for brazing on steel, cast iron, copper and brass. Active from 1400°F to 2000°F. Performs to AWS A5.31,Type FB3-F

| Part No. | Model / Product Description | UPC |
|---|---|---|
| 69080205 | A/S BRAZO FLUX 1#CAN X 12 | 662393004043 |
Replaces L-TEC "Brazo" Flux and All-state Brazaloy 5 1/2 Flux.