ALL-STATE BRAZALOY 1 FLUX

General purpose brazing flux.

Features

A blue powder general purpose brazing flux for cast iron, steel, brass, bronze and copper brazing. Active from 1400°F to 2000°F. Performs to AWS A.31,Type FB3-F