Print this page

OK Flux 10.10

OK Flux 10.10 is an agglomerated flux for ESW (electro-slag) cladding. Can be used for single or multi-layer cladding. However, it is requires a special welding head and a power source operating at least 1200 AMPS.

Features

OK Flux 10.10 is suitable for strip surfacing with stainless strips of the Cr, CrNi and CrNiMo types, with or without Nb-stabilization. The weldability, bead appearance and slag removal of OK Flux 10.10 are excellent.

OK Flux 10.10 together with OK Band 309L produces a 308L weld deposit analysis in one layer.

OK Flux 10.10 together with OK Band 309LNb produces a 347 weld deposit analysis in one layer.

OK Flux 10.10 together with OK Band 309LMo produces a 316L weld deposit analysis in one layer.

OK Flux 10.10
  • Industry
  • Petrochemical
  • Process
  • Welding Process
  • SAW (Sub Arc)

Classifications

Properties

Typical Properties
Typical Undiluted Weld Metal Analysis  
As Welded  
OK Band 309L  
C .03 %
Mn 1.2 %
Si 0.4 %
Cr 19 %
Ni 10 %
Mo 0.2 %
OK Band 309LMo on 2.25Cr1Mo  
C 0.02 %
Mn 1.1 %
Si 0.4 %
Cr 18 %
Ni 12.5 %
Mo 2.8 %
OK Band 309LNb on mild steel  
C 0.03 %
Mn 1.3 %
Si 0.50 %
Cr 19 %
Ni 10 %
Nb 0.4 %
OK Band 309LNb on 2.25Cr1Mo-steel  
C 0.02 %
Mn 1.20 %
Si 0.4 %
Cr 18.5 %
Ni 10 %

Part No.

Flux 10.10
Part No. Model / Product Description UPC
1010000000 OK FLUX 10.10 25KG BG 662303070595
101000000A OK FLUX 10.10 25KG BG 662303079659

SAW

Accessories

Depositions/Paramaters

Extra Info

Basicity Index: 4.0

Complementary Products

Seismic Data

All listed prices are in U.S. dollars and represent the Manufacturer's Suggested Retail Price (MSRP) for sale in the United States. Actual selling price will be determined by the Distributor. Prices are subject to change without notice.