Refrac-T-Back is a non-metallic ceramic material which is temporarily attached to the reverse side of a weld while helping to support a full penetration weld.
Refrac-T-Back is a non-metallic ceramic material which is temporarily attached to the reverse side of a weld while helping to support a full penetration weld. Individually sized and cut to a specific length, these disposable tiles are flexible and easily adaptable to many different weld configurations. The cost savings potential makes this an attractive alternative to arc gouging and rewelding full penetration welds.
The composition of this non-metallic material is an ideal alternative to steel or copper backing bars. The quality and consistency within the ceramic composition eliminates any concern for metallurgical mismatch in either the base material or weld metal. The density of such a material not only helps support and define the molten weld metal, but more importantly, effectively resists moisture pick-up that can seriously affect the weld deposit.

| Part No. | Model / Product Description | UPC |
|---|---|---|
| 693000002 | RTB GROOVED 1X1X1/4 | 662303042899 |
| 693000010 | RTB FLAT 1X1X1/4 | 662303042806 |
| 693000044 | RTB GROOVED 2X2X3/8 | 662303042851 |
| 693000051 | RTB FLAT 2X2X3/8 | 662303042813 |
| 693000127 | RTB ROUND 3/8X1 36/CT | 662303042875 |
| 693000135 | RTB ROUND 1/2X1 36/CT | 662303042882 |
| 693000184 | RTB TRIANGLE 1 - 60F | 662303042714 |
| 693000192 | RTB TRIANGLE 1 - 45F | 662303042738 |
| 693000200 | RTB TRIANGLE 1 -75F | 662303042752 |
| 693000226 | RTB 350R 1X1X1/4 36/CT | 662303042844 |
| 693000234 | RTB 215R 1X1X1/4 | 662303042820 |
| 693000267 | RTB 625R 2X1X1/4X3/8 16/CT | 662303042837 |
| 693000283 | RTB ROUND 1/4X1 36/CT | 662303042905 |
| 693000291 | RTB FBF 1X1X1/4 36/CT | 662303042868 |
Individual tiles are assembled on an adhesive tape which can then be fitted to any specific length. Individual tiles can also be purchased and used in conjunction with a metal tracking system. Once attached to the reverse side of the weldment, preheat can be utilized. The adhesive characteristics permit the weld to be preheated up to 500ºF (270ºC) without releasing. Following the weld completion, both the tiles and tape are easily removed, exposing a consistent uniform weld bead.
Selecting the proper ceramic is specific to a given weld joint design. Each welding process (SMAW, FCAW, MIG, etc.) necessitates a different technique to successfully utilize this material. Because of the many different ceramic tile configurations, careful evaluation is recommended prior to implementation.
Refrac-T-Back tape comes in a variety of styles and configurations. The cost saving advantages are easily justified in both reduced labor and increased productivity. Part numbers and package options make selection easy.
All listed prices are in U.S. dollars and represent the Manufacturer's Suggested Retail Price (MSRP) for sale in the United States. Actual selling price will be determined by the Distributor. Prices are subject to change without notice.