OK Autrod 13.20SC is designed to produce a 2-1/4% Cr and 1% Mo weld deposit to be used for welding process piping, heat exchangers, and pressure vessel fabrication. Used in combination with OK Flux 10.63 it meets step-cooling requirements.
ESAB’s OK Autrod 13.20SC is a copper-coated low alloy submerged arc wire designed for the welding of creep-resistant steel of the 2-½% Cr-1% Mo type. When combined with OK Flux 10.63, OK Autrod 13.20SC produces a metalurgically clean weld which is capable of meeting X-factor of less than 15 and J-factor of less than 120. This combination fulfills the stringent requirements for toughness after step cooling treatment of the weld metal. OK Autrod 13.20SC can also be combined with OK Flux 10.62 for applications not requiring step cooling treatment.
OK Autrod 13.20SC is used for welding process piping, heat exchangers, and pressure vessel fabrication.

| Typical Mechanical Properties | |
|---|---|
| OK 10.62 | |
| SR, 1 hr. @ 1275 °F (690°C) | |
| Tensile Strength | 90 ksi, 620 MPa |
| Yield Strength | 76 ksi, 525 MPa |
| Elongation in 2" | 25 % |
| CVN | 59 ft. -lbs. |
| Temperature | -20 °F, -29 °C |
| OK 10.63 | |
| SR, 1 hr. @ 1275 °F (690°C) | |
| Tensile Strength | 91 ksi, 630 MPa |
| Yield Strength | 77 ksi, 530 MPa |
| Elongation in 2" | 25 % |
| CVN | 37 ft. -lbs., 50 J |
| Temperature | -80 °F, -62 °C |
| Typical Undiluted Weld Metal Analysis | |
| OK 10.62 | |
| C | 0.08 % |
| Mn | 0.6 % |
| Si | 0.2 % |
| Cr | 2.0 % |
| Mo | 0.85 % |
| P | 0.025 max % |
| S | 0.015 max % |
| OK 10.63 | |
| C | 0.07 % |
| Mn | 0.6 % |
| Si | 0.2 % |
| Cr | 2.1 % |
| Mo | 1.0 % |
| P | 0.010 max % |
| S | 0.010 max % |
| Wire Chemistries | |
| C | 0.10 % |
| Mn | 0.55 % |
| Si | 0.15 % |
| P | 0.005 % |
| S | 0.006 % |
| Cr | 2.25 % |
| Mo | 0.95 % |
All listed prices are in U.S. dollars and represent the Manufacturer's Suggested Retail Price (MSRP) for sale in the United States. Actual selling price will be determined by the Distributor. Prices are subject to change without notice.