Print this page

SHIELD-BRIGHT 309H

Shield-Bright 309H was developed for out-of-position weld on 309H stainless where high temperature service is required.

Features

Shield-Bright 309H was developed for the welding of Type 309 and similar stainless steels. Its ferrite content, which is lower than Shield-Bright 309L, allows for joining carbon and low alloy steels provided the dilution is not too great and the service temperature is above 750ºF (399ºC) where creep strength properties are necessary.

Shield-Bright 309H was designed for welding in all positions and performs particularly well in the vertical position with excellent slag removal.

* This item is subject to Industry Alloy Surcharges

Shield-Bright 309H
  • Industry
  • Process
  • General Fabrication
  • Welding Process
  • FCAW (Flux Core)

Classifications

  • Classifications/Approvals

    • AWS A5.22; E309T1-1/T1-4
    • ASME II SFA 5.22 E309T1-1/T1-4
    • ASME IX F No. 6

Properties

Typical Properties
As Welded 75% Ar / 25% CO2  
Tensile Strength 90 ksi, 620 MPa
Yield Strength 70 ksi, 480 MPa
Elongation in 2" 35 %
Typical Undiluted Weld Metal Analysis  
As Welded CO2  
C 0.06 %
Mn 1.2 %
Si 0.8 %
Cr 24 %
Ni 13 %
Mo 0.1 %
Cu 0.1 %
Ferrite 13 FN
As Welded 75% Ar / 25% CO2  
C 0.06 %
Mn 1.3 %
Si 0.9 %
Cr 24.5 %
Ni 13 %
Mo 0.1 %
Cu 0.1 %
Ferrite 14 FN

Part No.

309H
Part No. Model / Product Description UPC
252200209 SB 309H 045X33#PSP VP 662303007621
252201082 SB 309H 1/16X33#PSP VP 662303008222

SAW

Accessories

Depositions/Paramaters

Deposition Table
Diameter Amps Volts Wire Feed Speed Deposition Rate Efficiency Electrical Stickout
.035 in, 0.9 mm 100 A 23 265 ipm, 6.7 cm/min 2.9 lbs./hr., 1.3 kg./hr. 83.9 % 1/2 - 1 inches, 12.5 - 25 mm
120 A 23 315 ipm, 8 cm/min 3.4 lbs./hr., 1.5 kg./hr. 81.4 % 1/2 - 1 inches, 12.5 - 25 mm
140 A 25 405 ipm, 10.3 cm/min 4.6 lbs./hr., 2.1 kg./hr. 82.6 % 1/2 - 1 inches, 12.5 - 25 mm
170 A 26 530 ipm, 13.5 cm/min 5.7 lbs./hr., 2.6 kg./hr. 81.8 % 1/2 - 1 inches, 12.5 - 25 mm
.045 in, 1.2 mm 130 A 25 227 ipm, 5.8 cm/min 4.25 lbs./hr., 1.9 kg./hr. 84 % 1/2 - 1 inches, 12.5 - 25 mm
165 A 26 341 ipm, 8.7 cm/min 6.14 lbs./hr., 2.8 kg./hr. 83 % 1/2 - 1 inches, 12.5 - 25 mm
190 A 28 445 ipm, 11.3 cm/min 8.08 lbs./hr., 3.7 kg./hr. 84 % 1/2 - 1 inches, 12.5 - 25 mm
220 A 30 567 ipm, 14.4 cm/min 10.24 lbs./hr., 4.6 kg./hr. 84 % 1/2 - 1 inches, 12.5 - 25 mm
1/16 in, 1.6 mm 170 A 25 154 ipm, 3.9 cm/min 5.34 lbs./hr., 2.4 kg./hr. 83 % 1/2 - 1 inches, 12.5 - 25 mm
210 A 27 193 ipm, 4.9 cm/min 6.89 lbs./hr., 3.1 kg./hr. 82.5 % 1/2 - 1 inches, 12.5 - 25 mm
250 A 28 243 ipm, 6.2 cm/min 8.57 lbs./hr., 3.9 kg./hr. 83 % 1/2 - 1 inches, 12.5 - 25 mm
300 A 29 321 ipm, 8.2 cm/min 11.43 lbs./hr., 5.2 kg./hr. 83 % 1/2 - 1 inches, 12.5 - 25 mm

Extra Info

Shielding Gas

75%Ar / 25%CO2 or 100%CO2

Complementary Products