Designed for flat and horizontal position welding using CO2 shielding gas, Dual Shield 700X provides high deposition rates, high efficiency and excellent performance.
Dual Shield 700X is a low slag - high deposition efficiency flux cored wire designed to join heavy structural steel components. Designed for flat and horizontal position welding using CO2 shielding gas, this X Series wire provides high deposition rates, high efficiency and excellent performance. Additionally, weld beads have a flat profile and a thin slag cover that is easily removed.
Applications include earth-moving equipment, heavy machinery and large steel components.

| As Welded | |
|---|---|
| Shielding Gas | CO2 |
| Yield Strength | 71 ksi, 490 MPa |
| Tensile Strength | 82 ksi, 565 MPa |
| Elongation (In 2", 51 mm) | 27 % |
| Typical Charpy V-Notch Impact Properties | |
| Shielding Gas | CO2 |
| Testing Temperature | |
| 0°F (-18°C) | 26 ft. - lbs., 35 J |
| -20°F (-29°C) | 20 ft. - lbs., 27 J |
| Typical Undiluted Weld Metal Analysis (%) | |
| Shielding Gas | CO2 |
| C | 0.04 |
| Mn | 1.1 |
| Si | 0.5 |
| P | 0.016 |
| S | 0.009 |
| Ni | 0.4 |
| Diameter | Amperage | Voltage | Wire Feed Speed | Deposition Rate | TTW |
|---|---|---|---|---|---|
| 1/16 in. | 170 A | 24.5 V | 150 ipm | 3/4" - 1 1/2" | |
| 197 A | 25.4 V | 190 ipm | 3/4" - 1 1/2" | ||
| 224 A | 26.2 V | 230 ipm | 3/4" - 1 1/2" | ||
| 251 A | 27.1 V | 270 ipm | 3/4" - 1 1/2" | ||
| 278 A | 27.9 V | 310 ipm | 3/4" - 1 1/2" | ||
| 305 A | 28.8 V | 350 ipm | 3/4" - 1 1/2" | ||
| 332 A | 29.6 V | 390 ipm | 3/4" - 1 1/2" | ||
| 359 A | 30.5 V | 430 ipm | 3/4" - 1 1/2" | ||
| 386 A | 31.3 V | 470 ipm | 3/4" - 1 1/2" | ||
| 413 A | 32.2 V | 510 ipm | 3/4" - 1 1/2" | ||
| 440 A | 33.0 V | 550 ipm | 19.4 | 3/4" - 1 1/2" | |
| 3/32 in. | 250 A | 26.0 V | 90 ipm | 3/4" - 1 1/2" | |
| 284 A | 26.9 V | 114 ipm | 3/4" - 1 1/2" | ||
| 318 A | 27.8 V | 137 ipm | 3/4" - 1 1/2" | ||
| 352 A | 28.7 V | 161 ipm | 3/4" - 1 1/2" | ||
| 386 A | 29.6 V | 184 ipm | 3/4" - 1 1/2" | ||
| 420 A | 30.5 V | 208 ipm | 3/4" - 1 1/2" | ||
| 454 A | 31.4 V | 231 ipm | 3/4" - 1 1/2" | ||
| 488 A | 32.3 V | 255 ipm | 3/4" - 1 1/2" | ||
| 522 A | 33.2 V | 278 ipm | 3/4" - 1 1/2" | ||
| 556 A | 34.1 V | 302 ipm | 3/4" - 1 1/2" | ||
| 590 A | 35.0 V | 325 ipm | 24.4 | 3/4" - 1 1/2" |