Print this page

Dual Shield II 711X

Dual Shield II 711X is an all-position flux cored wire that displays exceptional impact properties and toughness in combination with CO2 shielding gas.

Features

Dual Shield II 711X is an all-position flux cored wire that displays exceptional impact properties in combination with CO2 shielding gas. This flux cored wire was developed to join low and medium carbon steels where higher impacts and toughness are required. As with all X Series wires, Dual Shield II 711X offers higher top-end current levels for out-of-position welding, broader operating ranges and higher deposition rates in out-of-position applications.

Applications include construction, shipbuilding, rail car, light and heavy equipment, and general fabrication where exceptional impacts are required. Weld metal analysis is similar to Atom Arc 7018 and Atom Arc 7018-1.

Dual Shield II 711X
  • Industry
  • Civil Construction
  • Rail Road Car
  • General Fabrication
  • Shipbuilding
  • Welding Process
  • FCAW (Flux Core)

Classifications

  • Classifications/Approvals

    • AWS A5.20; E71T-1CJ/T-9CJ/T-12CJ
    • ABS 3SA,3YSA
    • D.N.V.- III YMS(H10)
    • CERTIFIED BY C.W.B.- CSA W48
    • ASME SFA 5.20
    • L.R. - 3S,3YS

Properties

Typical Properties
As Welded  
Shielding Gas CO2
Yield Strength 78 ksi, 540 MPa
Tensile Strength 86 ksi, 595 MPa
Elongation (In 2", 51 mm) 29 %
Typical Charpy V-Notch Impact Properties  
Shielding Gas CO2
Testing Temperature  
0°F (-18°C) 96 ft. - lbs., 130 J
-20°F (-29°C) 79 ft. - lbs., 107 J
-40°F (-40°C) 36 ft. - lbs., 49 J
Typical Undiluted Weld Metal Analysis (%)  
Shielding Gas CO2
C 0.04
Mn 1.4
Si 0.4
P 0.012
S 0.010

Part No.

711X
Part No. Model / Product Description UPC
245019005 DS II 711X 045X33#AWS 662303082116
245019013 DS II 711X 052X33#AWS 662303082123
245019021 DS II 711X 1/16X33#AWS 662303082130

SAW

Accessories

Depositions/Paramaters

Deposition Table Gas: CO2
Diameter Amperage Voltage Wire Feed Speed Deposition Rate TTW
0.045 in. 110 A 19.5 V 150 ipm 1/2" - 1"
122 A 20.2 V 178 ipm 1/2" - 1"
134 A 20.9 V 205 ipm 1/2" - 1"
146 A 21.6 V 233 ipm 1/2" - 1"
158 A 22.3 V 260 ipm 1/2" - 1"
170 A 23.0 V 288 ipm 1/2" - 1"
182 A 23.7 V 315 ipm 1/2" - 1"
194 A 24.4 V 343 ipm 1/2" - 1"
206 A 25.1 V 370 ipm 1/2" - 1"
218 A 25.8 V 398 ipm 1/2" - 1"
230 A 26.5 V 425 ipm 7.4 lbs./hr. 1/2" - 1"
0.052 in. 150 A 20.5 V 160 ipm 1/2" - 1"
160 A 21.1 V 181 ipm 1/2" - 1"
170 A 21.6 V 201 ipm 1/2" - 1"
180 A 22.2 V 222 ipm 1/2" - 1"
190 A 22.7 V 242 ipm 1/2" - 1"
200 A 23.3 V 263 ipm 1/2" - 1"
210 A 23.8 V 283 ipm 1/2" - 1"
220 A 24.4 V 304 ipm 1/2" - 1"
230 A 24.9 V 324 ipm 1/2" - 1"
240 A 25.5 V 345 ipm 1/2" - 1"
250 A 26.0 V 365 ipm 8.7 lbs./hr. 1/2" - 1"
1/16 in. 135 A 21.5 V 110 ipm 1/2" - 1"
146 A 22.0 V 123 ipm 1/2" - 1"
156 A 22.4 V 136 ipm 1/2" - 1"
167 A 22.9 V 149 ipm 1/2" - 1"
178 A 23.3 V 162 ipm 1/2" - 1"
189 A 23.8 V 175 ipm 1/2" - 1"
199 A 24.2 V 188 ipm 1/2" - 1"
210 A 24.7 V 201 ipm 1/2" - 1"
221 A 25.1 V 214 ipm 1/2" - 1"
231 A 25.6 V 227 ipm 1/2" - 1"
242 A 26.0 V 240 ipm 8.8 lbs./hr. 1/2" - 1"

Extra Info

DCEP

Complementary Products

Seismic Data