Arcaloy ER308/308H is a high carbon grade of 308 for higher temperature requirements. Can be used in combination with OK Flux 10.93 or 10.95.
Arcaloy 308H is a continuous, solid, corrosion-resistant, chromium-nickel wire for welding austenitic chromium-nickel alloys of the 18% Cr - 8% Ni type.
| C | 0.06 % |
|---|---|
| Mn | 1.8 % |
| Si | 0.8 % |
| P | 0.030 % |
| S | 0.020 % |
| Cr | 20.3 % |
| Ni | 10.0 % |
| Mo | 0.30 % |
| Cu | 0.30 % |