OK Band 309LNb

OK Band 309LNb is a stainless strip for single layer electroslag strip surfacing. Band 309LNb together with OK Flux 10.10 produces a 347 weld deposit analysis in one layer.

Features

Overlay can be used in temperatures exceeding 400C fir mild corrosion. Good resistance to general, pitting and inter-crystalline corrosion.

Former product name was OK Band 11.72

* This item is subject to Industry Alloy Surcharges

OK Band 309LNb
  • Industry
  • Pressure Vessel
  • Petrochemical
  • Welding Process
  • SAW (Sub Arc)
  • ESW (Electroslag)

Classifications

  • Classifications/Approvals

    • SFA/AWS A5.9 EQ309LNb

Properties

Typical Properties
C <0.02 %
Mn 1.8 %
Si <0.4 %
Cr 20.5 %
Ni 13.5 %
Mo 3.1 %

Part No.

Band 309LNb
Part No. Model / Product Description UPC
1172560300 ES OKBAND 11.72X60MMX30KG 662303073343

SAW

Accessories

Depositions/Paramaters

Recommended Welding Parameters and Deposition Data
Amps Volts Welding Parameters Deposition Rate
1250256 in/min (16 cm/min)51 lbs/h (23 kg/h), 555 inch²/h (0.035 m²/h)