OK Band 316L is a stainless welding strip for designed for cladding using submerged arc welding process. Band 309L together with OK Flux 10.05 and Band 316L produces a 316L deposit.

Features

Former product name was OK Band 11.63

* This item is subject to Industry Alloy Surcharges

OK Band 316L
  • Industry
  • Petrochemical
  • Pressure Vessel
  • Welding Process
  • SAW (Sub Arc)

Classifications

  • Classifications/Approvals

    • SFA/AWS A5.9 EQ316L

Properties

Typical Properties
C <0.03 %
Mn 1.8 %
Si 0.5 %
Cr 19.0 %
Ni 12.5 %
Mo 2.8 %

Part No.

Band 316L
Part No. Model / Product Description UPC
1163560200 ES OKBAND 316L 60MMX25KG CL 662303071073
1163560300 ES OKBAND 11.63X60MMX30KG 662303071080

SAW

Accessories

Depositions/Paramaters

Recommended Welding Parameters and Deposition Data
Amps Volts Welding Parameters Deposition Rate
750285 in/min (12 cm/min)31 lbs/h (14kg/h), 345 inch²/h (0.23 m²/h)