Arcaloy ER316L is a continuous, solid, corrosion-resistant, chromium-nickel-molybdenum wire for welding austenitic stainless alloys of he 18% Cr, 8% Ni, and 18 % Cr, 8% Ni, 3% Mo types. Arcaloy ER316L can be used in combination with OK Flux 10.93 or 10.94.
Arcaloy 316L has good general corrosion resistance. In particular, the alloy has very good corrosion resistance to corrosion in acid and chlorinated environments. The carbon content is limited to a maximum of 0.03% in order to reduce the possibility of formation of intergranular carbide precipitation.
| C | .016 % |
|---|---|
| Mn | 1.87 % |
| Si | .48 % |
| P | .019 % |
| S | .01 % |
| Cr | 19.32 % |
| Ni | 13.2 % |
| Mo | 2.25 % |
| N | .05 % |
| Other | Fe -Bal |