OK Band 347 is a stainless welding strip designed for cladding using submerged arc welding process. Band 309L together with OK Flux 10.05 and Band 347 produces a 347 deposit.
Former product name was OK Band 11.62
* This item is subject to Industry Alloy Surcharges

| C | <0.03 % |
|---|---|
| Mn | 1.8 % |
| Si | 0.5 % |
| Cr | 20.3 % |
| Ni | 10.0 % |
| Mo | <0.3 % |
| Part No. | Model / Product Description | UPC |
|---|---|---|
| 1162560200 | ES OKBAND 347 60MMX25KG CL | 662303073220 |
| 1162560300 | ES OKBAND 11.62X60MMX30KG | 662303070984 |
| 259967305 | ES OKBAND 11.62X60MMX25KG |
| Amps | Volts | Welding Parameters | Deposition Rate |
|---|---|---|---|
| 750 | 28 | 5 in/min (12 cm/min) | 31 lbs/h (14 kg/h), 345 inch²/h (0.23 m²/h) |