Print this page

ALLOY SHIELD 423L

Alloy Shield 423L is a tubular, composite metal cored wire designed for hard surfacing worn steel mill concast rolls. It produces 35-40 Rc hardness after heat treatment. Used in combination with 601 flux.

Features

Alloy Shield 423L is a "composite" submerged arc wire designed for buildup and repair of steel mill caster rolls. This specially formulated wire is intended to provide a softer as-welded deposit than the Alloy Shield 420 wire. The weld deposit resists softening after tempering above 900°F (482°C). Alloy Shield 423L is designed to operate in conjunction with OK Flux 601.

* This item is subject to Industry Alloy Surcharges

ALLOY SHIELD 423L
  • Industry
  • Steel Industry
  • Welding Process
  • SAW (Sub Arc)

Classifications

Properties

Typical Properties
Typical Mechanical Properties Utilizing OK Flux 601  
Hardness As Welded 37 Rc
Hardness Stress Relieved 7 hrs. @ 1050ºF (565ºC) 37 Rc
Typical All Weld Metal Analysis Utilizing OK Flux 601  
C 0.09 %
Mn 1.4 %
Si 0.6 %
Cr 11.9 %
Ni 0.9 %
Mo 1.3 %
V 0.2 %
Nb 0.4 %

Part No.

423L
Part No. Model / Product Description UPC
258076579 AS 423L 1/8X500#POP 662303008765
258076348 AS 423L 1/8X60#CL 662303072407

SAW

Accessories

Depositions/Paramaters

Extra Info

Complementary Products

Seismic Data

All listed prices are in U.S. dollars and represent the Manufacturer's Suggested Retail Price (MSRP) for sale in the United States. Actual selling price will be determined by the Distributor. Prices are subject to change without notice.