ARCALOY 625

Arcaloy ER625 is a Ni-Cr-Mo alloy designed for cladding iron and joining similar steels or dissimilar steels such as stainless and low alloy materials.

Features

Arcaloy ER625 is a Ni-Cr-Mo alloy designed for use for cladding iron and joining similar steels or dissimilar steels such as stainless and low alloy materials. The low iron content present in this product is advantageous to control dilution. The ER625 alloy provides maximum resistance to stress corrosion cracking, pitting and crevice corrosion.

* This item is subject to Industry Alloy Surcharges

ARCALOY 625
  • Industry
  • Process
  • Cryogenic
  • Petrochemical
  • Welding Process
  • GTAW (TIG)
  • GMAW (MIG)
  • SAW (Sub Arc)
  • SMAW (Stick)

Classifications

  • Classifications/Approvals

    • AWS A5.14; ERNiCrMo-3
    • ASME II SFA 5.14 ERNiCrMo-3
    • ASME IX F No. 43

Properties

Typical Properties
C 0.01 %
Mn 0.030 %
Si 0.059 %
P 0.004 %
S 0.002 %
Cr 22.5 %
Ni 65 %
Mo 8.7 %
Al 0.1 %
Ti 0.18 %
Cu .051 %
Nb 3.6 %
Cb 3.5 %
Fe 0.310 %

Part No.

625
Part No. Model / Product Description UPC
256196007 AB ER625 045X33#PSP 662303042325
256196015 AB ER625 035X33#PSP 662303050016

SAW

Accessories

Depositions/Paramaters

Extra Info

Arcaloy ER625 is a solid wire and is for welding Inconel 625®, UNS N06625, and similar alloys for service at high and cryogenic temperatures. It is one of the filler metals suitable for the welding of stainless steels containing 4% or more molybdenum. It is used welding 9% Ni steels and for dissimilar joints between nickel alloys, stainless and low alloy steels. It can also be used for cladding steels.
Depending upon its form, Arcaloy ER625 can be used in the MIG, TIG or submerged arc processes to name the three most common. In the case of the MIG (GMAW), spray, pulse or short-arc modes of transfer are used depending on the gas used. With this process, shielding gases of argon possibly with helium and very small quantites of oxygen or carbon dioxide are used. For TIG (GTAW), 100% argon or argon with some helium additions are used. A flux, such as OK Flux 10.16, is used with the larger sizes of Arcaloy ER625 for submerged-arc welding.