ARCALOY ER276

Arcaloy ER276 is a Ni-Cr-Mo alloy designed for joining or cladding where resistance to stress corrosion cracking, pitting and crevice corrosion is essential.

Features

Arcaloy ER276 is a Ni-Cr-Mo alloy designed for joining or cladding nickel based alloys and stainless steels. The higher Moly content offers maximum pitting and crevice corrosion protection.

* This item is subject to Industry Alloy Surcharges

ARCALOY ER276
  • Industry
  • Process
  • Pulp and Paper
  • Welding Process
  • GMAW (MIG)
  • GTAW (TIG)
  • SAW (Sub Arc)

Classifications

  • Classifications/Approvals

    • ASME IX F No. 44
    • ASME II SFA 5.14 ERNiCrMo-4
    • AWS A5.14; ERNiCrMo-4

Properties

Typical Properties
C 0.007 %
Mn 0.45 %
Si 0.05 %
P 0.007 %
S 0.002 %
Cr 16 %
Ni 58 %
Mo 16 %
Al 0.1 %
Co 0.02 %
V <0.01 %
Cu 0.01 %
Fe 5.7 %
W 3.8 %

Part No.

ER276
Part No. Model / Product Description UPC
256071705 AB ER276 1/16X36X10T/30CT INK 662303049881
256071713 AB ER276 3/32X36X10T/30CT INK 662393012079
256071721 AB ER276 1/8X36X10T/30CT INK 662393012123
256071739 AB ER276 035X30#PSP 662303049980
256071747 AB ER276 045X33#PSP 662303049997
256071754 AB ER276 1/16X30#PSP 662393012130

SAW

Accessories

Depositions/Paramaters

Extra Info

ER276 is a solid wire and is for welding Hastelloy C-276®, UNS N10276, and similar alloys. It is one of the filler metals suitable for the welding of stainless steels containing 4% or more molybdenum. It is used for dissimilar joints between nickel alloys, stainless and low alloy steels. It can also be used for cladding steels. Depending upon its form, ER276 can be used in the MIG, TIG or submerged arc processes to name the three most common. In the case of the MIG (GMAW), spray, pulse or short-arc modes of transfer are used depending on the gas used. With this process, shielding gases of argon possibly with helium and very small quantities of oxygen or carbon dioxide are used. For TIG (GTAW), 100% argon or argon with some helium additions are used. A flux, such as OK Flux 10.16, is used with the larger sizes of ER276 for submerged-arc welding.