OK Tigrod 309LSi has good general corrosion resistance. The higher silicon content improves the welding properties such as wetting.
OK Tigrod 309LSi is a bare, corrosion-resistant, chromium-nickel welding rod for welding of similar composition, wrought and cast steels of 23% Cr-12% Ni types. The alloy is also used for welding of buffer layers on CMn steels and welding of dissimilar joints. When using the wire for buffer layers and dissimilar joints, it is necessary to control the dilution of the weld.

| Yield Strength | 69 ksi, 475 MPa |
|---|---|
| Tensile Strength | 92 ksi, 635 MPa |
| Elongation in 2" | 32 % |
| Typical Charpy V-Notch Impact Properties | |
| Testing Temperature -76°F (-60°C) | 96 ft.-lbs, 130 J |
| Testing Temperature -166°F (-110°C) | 59 ft.-lbs, 80 J |
| Testing Temperature 68ºF (20ºC) | 111 ft.-lbs., 150 J |
| Typical wire analysis | |
| C | <0.03 % |
| Mn | 1.8 % |
| Si | 0.8 % |
| Cr | 24.0 % |
| Ni | 13.0 % |
| Mo | <0.3 % |
| Cu | <0.3 % |
| Part No. | Model / Product Description | UPC |
|---|---|---|
| 165116R15A | ES OK ER309LSI 1/16X39X11 E2 | 662303085056 |
| 165124R15A | ES OK ER309LSI 3/32X39X11 E2 | 000000000000 |
| 165132R15A | ES OK ER309LSI 1/8X39X11 E2 | 000000000000 |
| 165140R15A | ES OK ER309LSI 5/32X39X11 E2 | 000000000000 |
All listed prices are in U.S. dollars and represent the Manufacturer's Suggested Retail Price (MSRP) for sale in the United States. Actual selling price will be determined by the Distributor. Prices are subject to change without notice.