OK Autrod 309LSi

OK Autrod 309LSi has good general corrosion resistance. This high silicon MIG wire improves the wetting characteristics of the weld deposit.

Features

OK Autrod 309LSi is a continuous, solid, corrosion resistant chromium-nickel wire for welding of similar composition, wrought and cast steels of 23% Cr-12% Ni types. The alloy is also used for welding of buffer layers on CMn steels and welding of dissimilar joints. When using the wire for buffer layers and dissimilar joints it is necessary to control the dilution of the weld.

OK Autrod 309LSi
  • Industry
  • Shipbuilding
  • Automotive
  • Process
  • General Fabrication
  • Welding Process
  • GMAW (MIG)

Classifications

  • Classifications/Approvals

    • ASME SFA 5.9

Properties

Typical Properties
Yield Strength 64 ksi, 440 MPa
Tensile Strength 87 ksi, 600 MPa
Elongation in 2" 41 % %
Typical Charpy V-Notch Impact Properties  
Testing Temperature -76°F (-60°C) 96 ft.-lbs, 130 J
Testing Temperature -166°F (-110°C) 66 ft.-lbs, 90 J
Testing Temperature 68ºF (20ºC) 118 ft.-lbs., 160 J
Typical Undiluted Weld Metal Analysis  
C <0.03 %
Mn 1.8 %
Si 0.8 %
Cr 24.0 %
Ni 13.0 %
Mo <0.3 %
Cu <0.3 %

Part No.

Autrod 309LSi
Part No. Model / Product Description UPC
165108982A ES OK ER309LSI 030X33#BAWS 000000000000
165109932A ES OK ER309LSI 035X550#OMP 662303084875
165111932A ES OK ER309LSI 045X550#OMP 000000000000
165111982A ES OK ER309LSI 045X33#BAWS 000000000000
165116982A ES OK ER309LSI 1/16X33#BAWS 000000000000
165109982A ES OK ER309LSI 035X33#BAWS 662303077501

SAW

Accessories

Depositions/Paramaters

Spray Transfer Deposition Table
Diameter Wire Feed Speed Amps Volts Deposition Rate
0.030 in, 0.8 mm 157-669 ipm, 400-1700 cm/min 55-160 15-24 2.2-8.8 lbs./hr., 1.0-4.0 kg./hr.
0.035 in, 0.9 mm 138-709 ipm, 350-1800 cm/min 65-220 15-28 2.4-12 lbs./hr., 1.1-5.4 kg./hr.
0.040 in, 1.0 mm 157-630 ipm, 400-1600 cm/min 80-240 15-28 3.3-13.2 lbs./hr., 1.5-6.0 kg./hr.
0.045 in, 1.2 mm 118-551 ipm, 300-1400 cm/min 100-300 15-29 3.5-16.5 lbs./hr., 1.6-7.5 kg./hr.
Shortarc Transfer Deposition Table
Diameter Wire Feed Speed Amps Volts Deposition Rate
0.030 in, 0.8 mm 156-312 ipm, 396-792 cm/min 40-120 15-20 1.4-3.8 lbs./hr., 3.8 kg./hr.
0.035 in, 0.9 mm 156-312 ipm, 396-792 cm/min 60-140 15-21 1.6-5.4 lbs./hr., 0.73-2.45 kg./hr.
0.045 in, 1.2 mm 140-280 ipm, 356-711 cm/min 100-210 17-22 2.4-6.0 lbs./hr., 1.09-2.72 kg./hr.