OK Tigrod 308L is a bare, corrosion-resistant, chromium-nickel TIG rod. OK Tigrod 308L has a good general corrosion resistance. The alloy has a low carbon content which makes this alloy particularly recommended where there is a risk of intergranular corrosion.

Features

OK Tigrod 308L is widely used in the chemical and food processing industries as well as for pipes, tubes and boilers. Suitable for the joining of stainless steels of 18% Cr - 8% Ni-type with low carbon content and Nb-stabilized steels of the same type if the service temperature does not exceed 662°F (350ºC). Can also be used for welding of Cr steels except in sulphur-rich environments.

OK Tigrod 308L
  • Industry
  • Food and Beverage
  • General Fabrication
  • Process
  • Welding Process
  • GTAW (TIG)

Classifications

  • Classifications/Approvals

    • AWS A5.9; ER308L/ER308
    • ASME II SFA 5.9 ER308L/ER308
    • DnV
    • UDT
    • VdTUV
    • ASME IX F No. 6

Properties

Typical Properties
Yield Strength 65 ksi, 450 MPa
Tensile Strength 94 ksi, 645 MPa
Elongation in 2" 36 % %
Typical Charpy V-Notch Impact Properties  
Testing Temperature -112°F (-80°C) 100 ft.-lbs, 135 J
Testing Temperature -320ºF (-196ºC) 66 ft.-lbs., 90 J
Testing Temperature 68ºF (20ºC) 125 ft.-lbs., 170 J
Typical wire analysis  
C <0.03 %
Mn 1.8 %
Si 0.5 %
Cr 20.3 %
Ni 10.0 %
Mo <0.3 %
Cu <0.3 %

Part No.

Tigrod 308L
Part No. Model / Product Description UPC
161016R15A ES OK ER308L 1/16X39X11CT E2 000000000000
161024R15A ES OK ER308L 3/32X39X11CT E2 000000000000
161032R15A ES OK ER308L 1/8X39X11CT E2 000000000000
161040R15A ES OK ER308L 5/32X39X11CT E2 000000000000