OK Autrod 308LSi has good general corrosion resistance. This high silicon MIG wire improves wetting characteristics of the weld deposit.
OK Autrod 308LSi is a continuous, solid, corrosion-resistant, chromium-nickel wire for welding austenitic chromium-nickel alloys of the 18 Cr- 8% Ni type. The alloy has a low carbon content, making it particularly recommended where there is a risk of intergranular corrosion.

| Yield Strength | 54 ksi, 370 MPa |
|---|---|
| Tensile Strength | 90 ksi, 620 MPa |
| Elongation in 2" | 36 % % |
| Typical Charpy V-Notch Impact Properties | |
| Testing Temperature -76°F (-60°C) | 66 ft.-lbs, 90 J |
| Testing Temperature -320ºF (-196ºC) | 44 ft.-lbs., 60 J |
| Testing Temperature 68ºF (20ºC) | 81 ft.-lbs., 110 J |
| Typical Undiluted Weld Metal Analysis | |
| C | <0.03 % |
| Mn | 1.8 % |
| Si | 0.8 % |
| Cr | 20.3 % |
| Ni | 10 % |
| Mo | <0.3 % |
| Cu | <0.3 % |
| Part No. | Model / Product Description | UPC |
|---|---|---|
| 161208982A | ES OK ER308LSI 030X33#BAWS | 000000000000 |
| 161209932A | ES OK ER308LSI 035X550#OMP | 000000000000 |
| 161209982A | ES OK ER308LSI 035X33#BAWS | 662303082833 |
| 161211982A | ES OK ER308LSI 045X33#BAWS | 662303079871 |
| 161216982A | ES OK ER308LSI 1/16X33#BAWS | 000000000000 |
| 161211932A | ES OK ER308LSI 045X550#OMP | 662303076849 |
| Diameter | Wire Feed Speed | Amps | Volts | Deposition Rate |
|---|---|---|---|---|
| 0.030 in, 0.8 mm | 265-500 ipm, 673-1397 cm/min | 160-210 | 24-28 | 6.5-9.6 lbs./hr., 2.95-4.35 kg./hr. |
| 0.035 in, 0.9 mm | 240-468 ipm, 610-1189 cm/min | 170-255 | 24-30 | 7.8-12.7 lbs./hr., 3.54-5.76 kg./hr. |
| 0.045 in, 1.2 mm | 192-360 ipm, 488-914 cm/min | 200-300 | 24-30 | 6.8-13.6 lbs./hr., 3.08-6.17 kg./hr. |
| 1/16 in, 1.6 mm | 120-192 ipm, 305-488 cm/min | 215-325 | 24-32 | 7.3-14.5 lbs./hr., 3.31-6.58 kg./hr. |
| Diameter | Wire Feed Speed | Amps | Volts | Deposition Rate |
|---|---|---|---|---|
| 0.030 in, 0.8 mm | 156-312 ipm, 396-792 cm/min | 40-120 | 15-20 | 1.4-3.8 lbs./hr., 0.64-1.72 kg./hr. |
| 0.035 in, 0.9 mm | 156-312 ipm, 396-792 cm/min | 60-140 | 15-21 | 1.6-5.4 lbs./hr., 0.73-2.45 kg./hr. |
| 0.045 in, 1.2 mm | 140-280 ipm, 356-711 cm/min | 100-210 | 17-22 | 2.4-6.0 lbs./hr., 1.09-2.72 kg./hr. |
All listed prices are in U.S. dollars and represent the Manufacturer's Suggested Retail Price (MSRP) for sale in the United States. Actual selling price will be determined by the Distributor. Prices are subject to change without notice.