OK Flux 10.90 is a neutral, bonded flux specifically designed for welding nickel based alloys and also 9% nickel steel with wires such as ERNiCrMo-3 (Inconel 525®) and ERNiCrMo-4 (Hastalloy 276®) wires.
OK Flux 10.90 is a manganese adding, which reducres the risk of hot cracking. Good slag detachability and good bead appearance.

| OK Flux 10.90 | |
|---|---|
| Typical Mechanical Properties, As Welded | |
| Arcaloy 625 | |
| Tensile Strength | 104 ksi, 720 MPa |
| Yield Strength | 64 ksi, 441 MPa |
| Charpy at -320°F (-196°C) | 73 ft-lbs, 99 J |
| Typical Undiluted Weld Analysis, As Welded | |
| Arcaloy ER625 | |
| C | 0.009 % |
| Si | 0.2 % |
| Mn | 1.32 % |
| P | 0.013 % |
| S | 0.007 % |
| Cr | 21.2 % |
| Ni | 63 % |
| Mo | 8.4 % |
| Nb | 3 % |
| Fe | 2.5 % |
| Typical Undiluted Weld Metal Analysis, As Welded | |
| Arcaloy 276 | |
| Tensile Strength | 99 ksi, 681 MPa |
| Yield Strength | 72 ksi, 497 MPa |
| Charpy at -320°F (-196°C) | 46 ft-lbs, 63 J |
| Typical Undiluted Weld Analysis, As Welded | |
| Arcaloy 276 | |
| C | 0.011 % |
| Si | 0.16 % |
| Mn | 1.79 % |
| P | 0.009 % |
| S | 0.001 % |
| Cr | 15.6 % |
| Ni | Bal. |
| Mo | 13.9 % |
| Nb | 0.09 % |
| Fe | 6.7 % |
| Basicity Index: | 1.7 |
| Chemical Composition: | |
| SiO2 + TiO2 | 10 |
| Al2 + MnO | 240 |
| Fluorides | 45 |
| Flux Consumption | |
| (lb. Flux / lb. Wire) | |
| Voltage | DC+ |
| 26 | 0.5 |
| 30 | 0.6 |
| 34 | 0.8 |
| 38 | 1.0 |