Typical Properties
OK Flux 10.95  
Typical Mechanical Properties, As Welded  
ER308L  
Tensile Strength 78 ksi, 540 MPa
Yield Strength 58 ksi, 400 MPa
Elongation 40 %
CVN 65 ft-lbs, 88 J
Temperature 68 °F, 20 °C
CVN 37 ft-lbs, 50 J
Temperature -320 °F, -196 °C
Typical Undiluted Weld Metal Analysis, As Welded  
ER308L  
C 0.03 %
Mn 1.4 %
Si 0.6 %
Cr 20.0 %
Ni 11.0 %
Mo 0.1 %
N 0.06 %
FN 3
Typical Mechanical Properties, As Welded  
ER308H  
Tensile Strength 75 ksi, 520 MPa
Yield Strength 39 ksi, 270 MPa
Elongation 55 %
Typical Undiluted Weld Analysis, As Welded  
ER308H  
C 0.08 %
Mn 1.8 %
Si 0.4 %
Cr 20.5 %
Ni 10.0 %
Mo 0.1 %
N 0.05 %
FN 8
Typical Mechanical Properties, As Welded  
ER347  
Tensile Strength 90 ksi, 620 MPa
Yield Strength 66 ksi, 455 MPa
Elongation 38 %
CVN 74 ft-lbs, 100 J
Temperature 68 °F, 20 °C
CVN 22 ft-lbs, 30 J
Temperature -320 °F, -196 °C
Typical Undiluted Weld Analysis, As Welded  
ER347  
C 0.04 %
Mn 1.0 %
Si 0.5 %
Cr 19.0 %
Ni 10.0 %
Nb 0.5 %
FN 6
Typical Mechanical Properties, As Welded  
ER316L  
Tensile Strength 82 ksi, 565 MPa
Yield Strength 57 ksi, 390 MPa
Elongation 40 %
CVN 30 ft-lbs, 40 J
Temperature -320 °F, -196 °C
Typical Undiluted Weld Analysis, As Welded  
ER316L  
C 0.03 %
Mn 1.4 %
Si 0.6 %
Cr 18.5 %
Ni 11.6 %
Mo 2.7 %
N 0.04 %
FN 3

Part No.

Flux 10.95
Part No. Model / Product Description UPC
109500000A OK FLUX 10.95 25KG BG 662303081652

SAW

Accessories

Depositions/Paramaters

Extra Info

Basicity Index:1.7

Flux Consumption
(lb. Flux / lb. Wire)
VoltageDC+
260.5
300.6
340.8
381.0