ESAB MIG-6

ESAB MIG-6 is an ER70S-6 MIG wire suited for welding over heavier amounts of dirt,rust,or mill scale.

Features

ESAB MIG-6 contains higher levels of deoxidizers(manganese and silicon)as compared to a general purpose wire such as ESAB MIG-3. The high content of deoxidizers allow welding over heavier amounts of dirt,rust, and mill scale while providing a more fluid puddle and smoother bead profile.

ESAB MIG-6
  • Industry
  • Automotive
  • Mobile Machinery
  • Shipbuilding
  • Civil Construction
  • General Fabrication
  • Welding Process
  • GMAW (MIG)

Classifications

  • Classifications/Approvals

    • Certified by CWB to CSA W48
    • AWS SFA5.18; ER70S-6

Properties

Typical Properties
As Welded GMAW CO2  
Yield Strength 61 ksi, 424 MPa
Tensile Strength 75 ksi, 518 MPa
Elongation in 2" 28 %
As Welded GMAW 75% Ar / 25% CO2  
Yield Strength 70 ksi, 483 MPa
Tensile Strength 84 ksi, 583 MPa
Elongation in 2" 26 %
Typical Charpy V-Notch Impact Properties  
Testing Temperature -20°F (-29°C)  
As Welded GMAW CO2 57 ft.-lbs., 77 J
As Welded GMAW 75% Ar / 25% CO2 67 ft.-lbs., 91 J
Typical Undiluted Weld Metal Analysis  
GMAW CO2  
C 0.073 %
Mn 0.97 %
Si 0.51 %
P 0.009 %
S 0.013 %
GMAW 75% Ar / 25% CO2  
C 0.075 %
Mn 1.22 %
Si 0.67 %
P 0.010 %
S 0.014 %

Part No.

MIG-6
Part No. Model / Product Description UPC
1632C01 MIG-6 052X44#SP 2772#/PLT 662303520342
1632C04 MIG-6 030X44#SP 662303514808
1632C25 MIG-6 035X44#SP 2772#/PLT 662303518608
1632C27 MIG-6 045X44#SP 2772#/PLT 662303518615
1634C47 MIG-6 045X60#CL 662303517472
1638C04 MIG-6 030X33#SP 662303517021
1638C45 MIG-6 035X18KG/40#AWS 662303518158
1638C47 MIG-6 045X18KG/40#AWS 662303518165
1639C01 MIG-6 052X550#MP 2/PLT 662303516888
1639C41 MIG-6 052X900#MP 662303518530
1639C45 MIG-6 035X900#MP PBPLT 662303517540
1639C47 MIG-6 045X900#MP PBPLT 662303517564
1639C48 MIG-6 1/16X900#MP PB/PLT 662303521820
1639C65 MIG-6 035X550#MP 2/PLT 662303518233
1639C67 MIG-6 045X550#MP 2/PLT 662303518226
1639F05 MIG-6 035X550#MP 4/PLT 662303519605
163TC40 MIG-6 025X11#SP/44# 662303522544
163TC44 MIG-6 030X11#SP/44# 662303522551
163TC45 MIG-6 035X11#SP/44# 662303522568
163TC85 MIG-6 035X33#AWS 662303520007
163TC87 MIG-6 045X33#AWS 662303520618
163XF05 MIG-6 035X600#OMP PBPLT AB 662303521967
163XF07 MIG-6 045X600#OMP PBPLT AB 662303521974
163XF41 MIG-6 052X900#OMP PBPLT AB 662303668358
163XF45 MIG-6 035X900#OMP PBPLT AB 662303521615
163XF47 MIG-6 045X900#OMP PBPLT AB 662303521783
1638C44 MIG-6 030X18KG/40#AWS 662303080686
1638C45A MIG-6 035X60#SP 662303080082
1638C46 MIG-6 040X18KG/40#AWS 662303069469
1638C47A MIG-6 045X60#SP 662303080099
163UF65 MIG-6 035X550#OMP 2/PLT 662303081669
163UF67 MIG-6 045X550#OMP 2/PLT 662303081676

SAW

Accessories

Depositions/Paramaters

Extra Info

ESAB MIG-6 is used for welding carbon sheet steel and plate of various thicknesses. Typical applications include automotive, heavy equipment, structural pipe, and HVAC duct work.

Complementary Products

Seismic Data

All listed prices are in U.S. dollars and represent the Manufacturer's Suggested Retail Price (MSRP) for sale in the United States. Actual selling price will be determined by the Distributor. Prices are subject to change without notice.