Print this page

OK Aristorod 12.50 (ER70S-6)

OK AristoRod 12.50 is a manganese-silicon alloyed MIG wire used to weld carbon steels. It provides a highly fluid puddle for good wetting action and a high tolerance of rust and mill scale.

Features

OK AristoRod 12.50 is a MIG wire featuring ESAB’s proprietary ASC (Advanced Surface Characteristics) technology. The unique wire surface of AristoRod improves feedability and arc stability, provides extended corrosion resistance and arc starting properties, and reduces contact tip wear. AristoRod 12.50 contains sufficient levels of manganese and silicon to provide a fluid weld puddle with superb wetting action. The high levels of manganese and silicon also make AristoRod 12.50 a good choice for welding over moderate to high levels of rust and mill scale. Shielding gas choices for AristoRod 12.50 include 100% CO2, argon/CO2 mixtures, argon/O2 mixtures, and other argon based mixed gas blends. AristoRod 12.50 is used to weld carbon steels typically used in structural, automotive, agricultural and heavy equipment, and other general fabrication.

OK Aristorod 12.50
  • Welding Process
  • GMAW (MIG)

Classifications

  • Classifications/Approvals

    • CWB CSA W48; ER49S-6
    • ABS 3SA,3YSA
    • BV SA3YM
    • DNV III YMS
    • DB 42.039.29
    • AWS SFA5.18; ER70S-6
    • GL 3YS
    • LR 3S 3YS
    • VdTUV 10052

Properties

Typical Properties
Shielding Gas  
90% Ar/10% CO2  
Yield Strength 66 ksi
Tensile Strength 82 ksi
Elongation in 2" 27 %
Reduction of Area 56 %
CVN (@-20°F) 82
75% Ar/25% CO2  
Yield Strength 66 ksi
Tensile Strength 82 ksi
Elongation in 2" 28 %
Reduction of Area 61 %
CVN (@-20°F) 44
100% CO2  
Yield Strength 65 ksi
Tensile Strength 78 ksi
Elongation in 2" 25 %
Reduction of Area 70 %
CVN (@-20°F) 27
Typical Undiluted Weld Metal Analysis  
90% Ar/10% CO2  
C 0.08 %
Mn 1.22 %
Si 0.730 %
P 0.013 %
S 0.012 %
Cu 0.01 %
75% Ar/25% CO2  
C 0.08 %
Mn 1.19 %
Si 0.68 %
P 0.012 %
S 0.012 %
Cu 0.02 %
100% CO2  
C 0.07 %
Mn 1.00 %
Si 0.56 %
P 0.012 %
S 0.011 %
Cu 0.01 %

Part No.

OK Aristorod 12.50 (ER70S-6)
Part No. Model / Product Description UPC
1A5009949A OK ARISTOROD12.50 035X900#OMP 662303078508
1A5011949A OK ARISTOROD12.50 045X900#OMP 662303078522
1A5013949A OK ARISTOROD12.50 052X900#OMP 662303077365
1A5009691A OK ARISTOROD12.50 035X40#AWS 662303083762
1A5011691A OK ARISTOROD12.50 045X40#AWS 662303076054
1A5013691A OK ARISTOROD12.50 052X40#AWS 662303076061

SAW

Accessories

Depositions/Paramaters

Deposition Table
Electrode Diameter Amps Deposition Rate lbs./hr (kg/hr)
    98% Ar 2% O2 *98% Eff. 75% Ar 25% CO2 *96% Eff. Straight CO2 *96% Eff.
.030 in., 0.8 mm 75 2.0, 0.91 1.9, 0.86 1.8, 0.82
100 2.6, 1.18 2.6, 1.18 2.5, 1.13
150 4.1, 1.86 4.0, 1.81 3.9, 1.77
200 6.8, 3.08 6.7, 3.04 6.5, 2.95
.035 in., 0.9 mm 80 2.2, 1.00 2.1, 0.95 2.0, 0.91
100 2.7, 1.22 2.7, 1.22 2.6, 1.18
150 4.2, 1.90 4.1, 1.86 4.0, 1.81
200 6.2, 2.81 6.0, 2.72 5.9, 2.68
250 9.0, 4.08 8.8, 3.99 8.6, 3.90
.045 in., 1.2 mm 100 2.1, 0.95 2.0, 0.91 1.9, 0.86
125 2.8, 1.27 2.8, 1.27 2.7, 1.22
150 3.6, 1.63 3.5, 1.59 3.4, 1.54
200 5.6, 2.54 5.5, 2.49 5.3, 2.40
250 7.8, 3.58 7.6, 3.45 7.4, 3.36
300 10.2, 4.63 10.0, 4.53 9.7, 4.40
350 13.2, 5.99 12.9, 5.85 12.5, 5.67
1/16 in., 1.6 mm 250 6.5, 2.95 6.4, 2.90 6.2, 2.81
275 7.7, 3.49 7.6, 3.45 7.3, 3.31
300 9.0, 4.08 8.8, 3.99 8.5, 3.86
350 11.3, 5.13 11.0, 4.99 10.7, 4.85
400 14.0, 6.35 13.7, 6.21 13.3, 6.03
450 17.4, 7.89 17.1, 7.76 16.5, 7.48

Extra Info