Sureweld 70 LA-2 contains a special lime coating which permits trouble-free welds on "difficult" steels .
Sureweld 70 LA-2 contains a special lime coating which permits trouble-free welds on "difficult" steels such as high-carbon, alloy, high-sulfur, free-machining, and cold-rolled steels. High amperages with corresponding high deposition rates make it more economical than conventional types on heavy work.

| As Welded | |
|---|---|
| Yield Strength | 71 ksi, 495 MPa |
| Tensile Strength | 83 ksi, 575 MPa |
| Reduction in Area | 75 % |
| Elongation in 2" | 28 % |
| Typical Charpy V-Notch Impact Properties | |
| Testing Temperature -20ºF (-29ºC) | |
| As Welded | 35 ft.-lbs., 47 J |
| Typical Undiluted Weld Metal Analysis | |
| C | 0.07 % |
| Mn | 0.9 % |
| Si | 0.5 % |
| P | 0.007 % |
| S | 0.016 % |
| Part No. | Model / Product Description | UPC |
|---|---|---|
| 811002195 | SW 70 LA-2 3/32X14X50#HS | 662303031442 |
| 811002203 | SW 70 LA-2 5/32X14X50#HS | 662303031459 |
| 811010297 | SW 70 LA-2 3/16X14X50#HS | 662303031497 |
| 811040674 | SW 70 LA-2 1/8X14X50#HS | 662303031510 |
| 811002104 | SW 70 LA-2 1/8X14X10#HS | 662303025373 |
| 811002112 | SW 70 LA-2 5/32X14X10#HS | 662303031428 |
| 811010347 | SW 70 LA-2 3/32X14X10#HS | 662303031503 |
| Diameter | Optimal Amperage | Range Amperage | Deposition Rate | Efficiency |
|---|---|---|---|---|
| 3/32 in, 2.4 mm | 75 A | 70 - 100 | 1.6 lbs./hr., 0.7 kg./hr. | 73 % |
| 1/8 in, 3.2 mm | 100 A | 110 - 140 | 1.7 lbs./hr., 0.8 kg./hr. | 63.9 % |
| 130 A | 110 - 140 | 2.3 lbs./hr., 1 kg./hr. | 65.8 % | |
| 5/32 in, 4.0 mm | 140 A | 140 - 200 | 3 lbs./hr., 1.4 kg./hr. | 70.5 % |
| 160 A | 140 - 200 | 3.2 lbs./hr., 1.5 kg./hr. | 69.1 % | |
| 190 A | 140 - 200 | 3.6 lbs./hr., 1.6 kg./hr. | 66 % | |
| 3/16 in, 4.8 mm | 175 A | 175 - 250 | 3.8 lbs./hr., 1.7 kg./hr. | 71 % |
| 200 A | 175 - 250 | 4.2 lbs./hr., 1.9 kg./hr. | 71 % | |
| 225 A | 175 - 250 | 4.4 lbs./hr., 2 kg./hr. | 70 % | |
| 250 A | 175 - 250 | 4.8 lbs./hr., 2.2 kg./hr. | 65.8 % | |
| 1/4 in, 6.4 mm | 250 A | 300 - 350 | 5.9 lbs./hr., 2.7 kg./hr. | 74.5 % |
| 275 A | 300 - 350 | 6.4 lbs./hr., 2.9 kg./hr. | 74.1 % | |
| 300 A | 300 - 350 | 6.8 lbs./hr., 3.1 kg./hr. | 73.2 % | |
| 350 A | 300 - 350 | 7.6 lbs./hr., 3.4 kg./hr. | 71.5 % |