Print this page

Coreweld 77-HS

Coreweld 77-HS is a metal-cored wire designed to run at faster travel speeds, higher deposition rates and leave very few silica islands.

Features

Coreweld 77-HS is a metal-cored wire designed to run at faster travel speeds, higher deposition rates and leave very few silica islands. This metal cored wire is ideal for robotic applications. Optimal performance is achieved with 90% Argon / 10% CO2 shielding gas.

Classifications

Properties

Typical Properties
As Welded 90% Ar / 10% CO2  
Yield Strength 63 ksi, 435 MPa
Tensile Strength 78 ksi, 535 MPa
Elongation in 2" (51 mm) 29 %
Reduction of Area 58 %
Diffusible Hydrogen 5 mL/100g
As Welded 75% Ar / 25% CO2  
Yield Strength 62 ksi, 430 MPa
Tensile Strength 77 ksi, 530 MPa
Reduction in Area 29 %
Elongation in 2" 60 %
Diffusible Hydrogen 5 mL/100g
Typical Charpy V-Notch Impact Properties  
Testing Temperature -20ºF (-29ºC)  
As Welded 75% Ar / 25% CO2 31 ft.-lbs., 42 J
As Welded 90% Ar / 10% CO2 35 ft.-lbs., 47 J
Typical Undiluted Weld Metal Analysis  
75% Ar / 25% CO2  
C 0.04 %
Mn 0.9 %
Si 0.7 %
P 0.012 %
S 0.018 %
Cr 0.05 %
Ni 0.1 %
Mo 0.1 %
90% Ar / 10% CO2  
C 0.04 %
Mn 1.0 %
Si 0.8 %
P 0.012 %
S 0.017 %
Cr 0.05 %
Ni 0.1 %
Mo 0.1 %

Part No.

77-HS
Part No. Model / Product Description UPC
243414000 CW 77-HS 045X33#AWS 662303073954
243414018 CW 77-HS 052X33#AWS 662303073947
243414026 CW 77-HS 1/16X33#AWS 662303073961

SAW

Accessories

Depositions/Paramaters

Deposition Table
Shielding Gas Diameter Amps Volts Wire Feed Speed
75% Ar / CO2 0.045 in, 1.2 mm 195 A 26 V 240 ipm, 609.6 cm/min
230 A 28 V 300 ipm, 762 cm/min
260 A 29 V 350 ipm, 889 cm/min
340 A 32 V 500 ipm, 1270 cm/min
370 A 33 V 550 ipm, 1397 cm/min
0.052 in, 1.4 mm 200 A 26 V 190 ipm, 482.6 cm/min
240 A 27 V 250 ipm, 635 cm/min

Extra Info

Shielding Gas

90% Argon / 10% CO2

Complementary Products

Seismic Data