ARCALOY ER308L

Arcaloy ER308L is a low carbon grade of 308 designed for MIG or TIG of stainless steels such as AISI 301, 304, 304L steels. SPECIAL ORDER ONLY

Features

Arcaloy ER308L has good general corrosion resistance. This alloy has a low carbon content which makes this alloy particularly recommended where there is a risk of intergranular corrosion. Arcaloy ER308L is also for joining 18% Cr - 8% Ni type and Nb-stabilized steels of the same type, assuming the service temperature will not exceed 662°F (350°C).

* This item is subject to Industry Alloy Surcharges

ARCALOY ER308L
  • Industry
  • Food and Beverage
  • Shipbuilding
  • Automotive
  • General Fabrication
  • Process
  • Welding Process
  • GMAW (MIG)
  • GTAW (TIG)

Classifications

  • Classifications/Approvals

    • ASME II SFA 5.9 ER308/308L
    • AWS A5.9; ER308/308L
    • Certified by CWB - AWS A5.9; ER308/308L
    • ASME IX F No. 6
    • QPL-19933; MIL-308L
    • A.B.S.- AWS A5.9; ER308/308L

Properties

Typical Properties
GTAW using 100% Argon  
Yield Strength 60 ksi, 410 MPa
Tensile Strength 88 ksi, 605 MPa
Elongation in 2" 43 %
Impact Toughness at -320ºF (-196ºC)  
Absorbed Energy 80 ft.-lbs., 110 J
Lateral Expansion 53 mils, 1.35 mm
Typical Chemical Analysis  
C 0.015 %
Mn 1.7 %
Si 0.45 %
S 0.01 %
Cr 20 %
Ni 10 %
Mo 0.1 %
Cu 0.15 %
Ferrite 9 FN

Part No.

ER308L
Part No. Model / Product Description UPC
256011834 AB ER308L 1/16X36X10#T/30CTINK 662303044633
256011842 AB ER308L 3/32X36X10T/30CT INK 662303030704
256011859 AB ER308L 1/8X36X10#T/30CT INK 662393008720
256011891 AB ER308L 5/32X36X10T/30CT INK 662303075262
257011122 AB ER308L 1/16X60#CL 662303008345
257011825 AB ER308L 1/8X60#CL 662303008352
257013326 AB ER308L 3/32X60#CL 662303008369
258011113 AB ER308L 1/16X33#PSP 662303027391
258013028 AB ER308L 030X10#PSP/60CT 662303027353
258013036 AB ER308L 030X33#PSP 662303030995
258013515 AB ER308L 035X33#BAWS 662303027377
258013523 AB ER308L 035X10#PSP/60CT 662303027360
258014513 AB ER308L 045X33#BAWS 662303027384
258023456 AB ER308L 045X10#PSP/60CT 662303043353

SAW

Accessories

Depositions/Paramaters

Short Circuit Transfer Table
Diameter Wire Feed Speed AMPS Volts Deposition Rate
.030 in., 0.8 mm 156-312 ipm, 396-792 cm/min 40-120 15-20 1.4-3.8 lbs./hr., 0.64-1.72 kg/hr
.035 in., 0.9 mm 156-312 ipm, 396-792 cm/min 60-140 15-21 1.6-5.4 lbs./hr., 0.73-2.45 kg/hr
.045 in., 1.2 mm 140-280 ipm, 356-711 cm/min 100-210 17-22 2.4-6.0 lbs./hr., 1.09-2.72 kg/hr
Spray Arc Transfer Table
Diameter Wire Feed Speed DCEP (Electrode Positive) Volts Deposition Rate
.030 in., 0.8 mm 265-550 ipm, 673-1397 cm/min 160-210 24-28 6.5-9.6 lbs./hr., 2.95-4.35 kg./hr.
.035 in., 0.9 mm 240-468 ipm, 610-1189 cm/min 170-255 24-30 7.8-12.7 lbs./hr., 3.54-5.76 kg./hr.
.045 in., 1.2 mm 192-360 ipm, 488-914 cm/min 200-300 24-30 6.8-13.6 lbs./hr., 3.08-6.17 kg./hr.
.062 in., 1.6 mm 120-192 ipm, 305-488 cm/min 215-325 24-32 7.3-14.5 lbs./hr., 3.31-6.58 kg./hr.