Arcaloy ER308/308H has good corrosion resistance in high temperature service.
Arcaloy ER308/308H is a continuous, solid, corrosion-resistant, chromium-nickel wire for welding austenitic chromium-nickel alloys of the 18% Cr-8% Ni type. Arcaloy ER308/308H has good general corrosion resistance.
* This item is subject to Industry Alloy Surcharges

| C | 0.05 % |
|---|---|
| Mn | 1.7 % |
| Si | 0.4 % |
| Cr | 20 % |
| Ni | 9.9 % |
| Mo | 0.05 % |
| Cu | 0.1 % |
| Ferrite | 7 FN |
| Part No. | Model / Product Description | UPC |
|---|---|---|
| 257015800 | AB ER308/308H 045X33#BAWS | 662303049560 |
| 257015826 | AB ER308/308H 035X33#BAWS | 662303034955 |
| 256021080 | AB ER308/308H 3/32X36X10/30INK | 662303078966 |
| 256021098 | AB ER308/308H 1/8X36X10/30INK | 662303078973 |
| 257015834 | AB ER308/308H 3/32X60#CL | 662303081645 |
| Diameter | Wire Feed Speed | Amps | Volts | Deposition Rate |
|---|---|---|---|---|
| .030 in, 0.8 mm | 265-550 ipm, 673-1397 cm/min | 160-210 | 24-28 | 6.5-9.6 lbs./hr., 2.95-4.35 kg./hr. |
| .035 in, 0.9 mm | 240-468 ipm, 610-1189 cm/min | 170-255 | 24-30 | 7.8-12.7 lbs./hr., 3.54-5.76 kg./hr. |
| .045 in, 1.2 mm | 192-360 ipm, 488-914 cm/min | 200-300 | 24-30 | 6.8-13.6 lbs./hr., 3.08-6.17 kg./hr. |
| .062 in, 1.6 mm | 120-192 ipm, 305-488 cm/min | 215-325 | 24-32 | 7.3-14.5 lbs./hr., 3.31-6.58 kg./hr. |
| Diameter | Wire Feed Speed | Amps | Volts | Deposition Rate |
|---|---|---|---|---|
| .030 in, 0.8 mm | 156-312 ipm, 396-792 cm/min | 40-120 | 15-20 | 1.4-3.8 lbs./hr., 0.64-1.72 kg./hr. |
| .035 in, 0.9 mm | 156-312 ipm, 396-792 cm/min | 60-140 | 15-21 | 1.6-5.4 lbs./hr., 0.73-2.45 kg./hr. |
| .045 in, 1.2 mm | 140-280 ipm, 356-711 cm/min | 100-210 | 17-22 | 2.4-6.0 lbs./hr., 1.09-2.72 kg./hr. |