Print this page

OK Tigrod 308LSi

OK Tigrod 308LSi has good general corrosion resistance. This high silicon Tigrod improves the welding properties such as wetting.

Features

OK Tigrod 308LSi
  • Industry
  • Process
  • General Fabrication
  • Food and Beverage
  • Welding Process
  • GTAW (TIG)

Classifications

  • Classifications/Approvals

    • AWS A5.9; ER308Si/308LSi
    • VdTUV
    • UDT
    • DNV
    • ASME II SFA 5.9 ER308Si/308LSi
    • ASME IX F No. 6
    • DEUTSCHE BAHN

Properties

Typical Properties
Yield Strength 74 ksi, 510 MPa
Tensile Strength 81 ksi, 555 MPa
Elongation in 2" 36 %
Typical Charpy V-Notch Impact Properties  
Testing Temperature -76°F (-60°C) 111 ft.-lbs, 150 J
Testing Temperature -166°F (-110°C) 103 ft.-lbs, 140 J
Testing Temperature -320ºF (-196ºC) 74 ft.-lbs., 100 J
Testing Temperature 68ºF (20ºC) 125 ft.-lbs., 170 J
Typical wire analysis  
C <0.03 %
Mn 1.8 %
Si 0.8 %
Cr 20.3 %
Ni 10.0 %
Mo <0.3 %
Cu <0.3 %

Part No.

Tigrod 308LSi
Part No. Model / Product Description UPC
161216R15A ES OK ER308LSI 1/16X39X11 E2 000000000000
161224R15A ES OK ER308LSI 3/32X39X11 E2 662303077648
161232R15A ES OK ER308LSI 1/8X39X11 E2 000000000000
161240R15A ES OK ER308LSI 5/32X39X11 E2 000000000000

SAW

Accessories

Depositions/Paramaters

Extra Info

Complementary Products

Seismic Data

All listed prices are in U.S. dollars and represent the Manufacturer's Suggested Retail Price (MSRP) for sale in the United States. Actual selling price will be determined by the Distributor. Prices are subject to change without notice.