Print this page

ARCALOY ER309L

Arcaloy ER309L is a low carbon grade of 309 for MIG or TIG welding.

Features

Arcaloy ER309L is a continuous, solid, corrosion-resistant, chromium-nickel wire for welding similar steels, wrought and cast steels of 23% Cr - 12% Ni types. The alloy is also used for welding of buffer layers on CMn steels and welding of dissimilar joints. When using the wire for buffer layers and dissimilar joints it is necessary to control the dilution of the weld.

* This item is subject to Industry Alloy Surcharges

ARCALOY ER309L
  • Industry
  • Process
  • General Fabrication
  • Automotive
  • Shipbuilding
  • Welding Process
  • GTAW (TIG)
  • GMAW (MIG)

Classifications

  • Classifications/Approvals

    • AWS A5.9; ER309/309L
    • CERTIFIED BY C.W.B.- AWS A5.9
    • A.B.S.- AWS A5.9; ER309/309L
    • QPL-19933; MIL-309
    • ASME II SFA 5.9 ER309/309L
    • ASME IX F No. 6

Properties

Typical Properties
GTAW using 100% Argon  
Yield Strength 60 ksi, 410 MPa
Tensile Strength 85 ksi, 590 MPa
Elongation in 2" 34 %
Typical Chemical Analysis  
C 0.02 %
Mn 1.8 %
Si 0.45 %
S 0.01 %
Cr 23.5 %
Ni 13.8 %
Mo 0.1 %
Cu 0.15 %
Ferrite 9 FN

Part No.

ER309L
Part No. Model / Product Description UPC
256031196 AB ER309L 5/32X36X10T/30CT INK 662303075255
256031816 AB ER309L 1/8X36X50#CT 662303026745
258013507 AB ER309L 035X33#PSP 662303076580
259602191 AB ER309L 1/16X18X10#CT F1 662303519667
256031139 AB ER309L 1/16X36X10T/30CT INK 662303044640
256031147 AB ER309L 3/32X36X10T/30CT INK 662303030766
256031154 AB ER309L 1/8X36X10T/30CT INK 662303030773
256071655 AB ER309L 035X10#PSP/60CT 662303043360
256071663 AB ER309L 045X10#PSP/60CT 662303043377
257031120 AB ER309L 1/16X60#CL 662303027209
257031823 AB ER309L 1/8X60#CL 662303008437
257033324 AB ER309L 3/32X60#CL 662303008444
257035329 AB ER309L 5/32X60#CL 662303027223
257035626 AB ER309L 5/64X60#CL 662303027216
258031111 AB ER309L 1/16X33#PSP 662303027551
258033026 AB ER309L 030X10#PSP/60CT 662303027537
258033513 AB ER309L 035X33#BAWS 662303026424
258034511 AB ER309L 045X33#BAWS 662303027544
258075829 AB ER309L 1/16X36X10#T 662303666934
259600328 AB ER309L 1/16X36X10#CT F2 662303667450
259601185 AB ER309L 3/32X36X10#CT F2 662303519148
257033332 AB ER309 3/32X60#CL 662303666927

SAW

Accessories

Depositions/Paramaters

Short Circuit Transfer Table
Diameter Wire Feed Speed AMPS Volts Deposition Rate
.030 in., 0.8 mm 156-312 ipm, 396-792 cm/min 40-120 15-20 1.4-3.8 lbs./hr., 0.64-1.72 kg/hr
.035 in., 0.9 mm 156-312 ipm, 396-792 cm/min 60-140 15-21 1.6-5.4 lbs./hr., 0.73-2.45 kg/hr
.045 in., 1.2 mm 140-280 ipm, 356-711 cm/min 100-210 17-22 2.4-6.0 lbs./hr., 1.09-2.72 kg/hr
Spray Arc Transfer Table
Diameter Wire Feed Speed DCEP (Electrode Positive) Volts Deposition Rate
.030 in., 0.8 mm 265-550 ipm, 673-1397 cm/min 160-210 24-28 6.5-9.6 lbs./hr., 2.95-4.35 kg./hr.
.035 in., 0.9 mm 240-468 ipm, 610-1189 cm/min 170-255 24-30 7.8-12.7 lbs./hr., 3.54-5.76 kg./hr.
.045 in., 1.2 mm 192-360 ipm, 488-914 cm/min 200-300 24-30 6.8-13.6 lbs./hr., 3.08-6.17 kg./hr.
.062 in., 1.6 mm 120-192 ipm, 305-488 cm/min 215-325 24-32 7.3-14.5 lbs./hr., 3.31-6.58 kg./hr.

Extra Info

Complementary Products

Seismic Data