Print this page

OK Tigrod 309LSi

OK Tigrod 309LSi has good general corrosion resistance. The higher silicon content improves the welding properties such as wetting.

Features

OK Tigrod 309LSi is a bare, corrosion-resistant, chromium-nickel welding rod for welding of similar composition, wrought and cast steels of 23% Cr-12% Ni types. The alloy is also used for welding of buffer layers on CMn steels and welding of dissimilar joints. When using the wire for buffer layers and dissimilar joints, it is necessary to control the dilution of the weld.

OK Tigrod 309LSi
  • Welding Process
  • GTAW (TIG)

Classifications

  • Classifications/Approvals

    • AWS A5.9; ER309Si/309LSi
    • VdTUV
    • ASME II SFA 5.9 ER309LSi/ER309Si
    • UDT

Properties

Typical Properties
Yield Strength 69 ksi, 475 MPa
Tensile Strength 92 ksi, 635 MPa
Elongation in 2" 32 %
Typical Charpy V-Notch Impact Properties  
Testing Temperature -76°F (-60°C) 96 ft.-lbs, 130 J
Testing Temperature -166°F (-110°C) 59 ft.-lbs, 80 J
Testing Temperature 68ºF (20ºC) 111 ft.-lbs., 150 J
Typical wire analysis  
C <0.03 %
Mn 1.8 %
Si 0.8 %
Cr 24.0 %
Ni 13.0 %
Mo <0.3 %
Cu <0.3 %

Part No.

Tigrod 309LSi
Part No. Model / Product Description UPC
165116R15A ES OK ER309LSI 1/16X39X11 E2 662303085056
165124R15A ES OK ER309LSI 3/32X39X11 E2 000000000000
165132R15A ES OK ER309LSI 1/8X39X11 E2 000000000000
165140R15A ES OK ER309LSI 5/32X39X11 E2 000000000000