Print this page

ARCALOY ER312

Arcaloy ER312 is used for welding stainless steels to mild steels and for welding high strength steels difficult to weld with ferritic electrodes.

Features

The weld deposit produces high tensile strength and good resistance to abrasion.

* This item is subject to Industry Alloy Surcharges

ARCALOY ER312
  • Industry
  • Pulp and Paper
  • General Fabrication
  • Petrochemical
  • Welding Process
  • GMAW (MIG)
  • GTAW (TIG)

Classifications

  • Classifications/Approvals

    • AWS A5.9; ER312
    • ASME II SFA 5.9 ER312
    • ASME IX F No. 6
    • QPL-19933; MIL-312

Properties

Typical Properties
C 0.1 %
Mn 1.8 %
Si 0.45 %
Cr 30 %
Ni 9 %
Mo 0.2 %
Cu 0.2 %
Ferrite 70 FN

Part No.

ER312
Part No. Model / Product Description UPC
256072604 AB ER312 1/16X36X10T/30CT INK 662303049140
256072612 AB ER312 3/32X36X10T/30CT INK 662303049157
256072620 AB ER312 1/8X36X10T/30CT INK 662303049164
257053322 AB ER312 3/32X60#CL 662303008475
257055624 AB ER312 5/64X60#CL 662393014042
090370 ER312 1/16 X 36 INK PRINTED  

SAW

Accessories

Depositions/Paramaters

Spray Transfer Deposition Table
Diameter Wire Feed Speed Amps Volts Deposition Rate
.030 in, 0.8 mm 265-550 ipm, 673-1397 cm/min 160-210 24-28 6.5-9.6 lbs./hr., 2.95-4.35 kg./hr.
.035 in, 0.9 mm 240-468 ipm, 610-1189 cm/min 170-255 24-30 1.7-12.7 lbs./hr., 3.54-5.76 kg./hr.
.045 in, 1.2 mm 192-360 ipm, 488-914 cm/min 200-300 24-30 6.8-13.6 lbs./hr., 3.08-6.17 kg./hr.
.062 in, 1.6 mm 120-192 ipm, 305-488 cm/min 215-325 24-32 7.3-14.5 lbs./hr., 3.31-6.58 kg./hr.
Shortarc Transfer Deposition Table
Diameter Wire Feed Speed Amps Volts Deposition Rate
.030 in, 0.8 mm 156-312 ipm, 396-795 cm/min 40-120 15-20 1.4-3.8 lbs./hr., 0.64-1.72 kg./hr.
.035 in, 0.9 mm 156-312 ipm, 396-792 cm/min 60-140 15-21 1.6-5.4 lbs./hr., 0.73-2.45 kg./hr.
.045 in, 1.2 mm 140-280 ipm, 356-711 cm/min 100-210 17-22 2.4-6.0 lbs./hr., 1.09-2.72 kg./hr.

Extra Info

Arcaloy ER312 is a solid wire and is for welding dissimilar joints, in particular where there is a high carbon content. With its high potential ferrite content, greater dilution by a non-stainless steel base metal is possible. Multi-pass welds can have beads with low base metal dilution in them therefore having a very high in ferrite content. This high ferrite can become brittle at high temperature and even with a high interpass temperature for a long period of time. Its high chromium content gives scaling resistance up to about 2000ºF (1100ºC). Depending upon its form, Arcaloy ER312 can be used in the MIG or TIG processes. In the case of the MIG (GMAW), spray, pulse or short-arc modes of transfer are used depending on the gas used. With this process, shielding gases or argon with 1 or 2% oxygen are commonly used for 'spray' and a mixture of 90% helium - 7.5% argon - 2.5% carbon dioxide is used for 'short-arc'.
For TIG (GTAW), 100% argon or argon with some helium additions are used.